所有产品
KM-027无PFAS版本可用

AF + UV Weatherable HC

Triple-function UV-curable coating combining antifouling, hard coating, and UV weatherability. Designed for outdoor display and automotive applications requiring long-term durability against UV degradation and surface fouling.

折射率范围n = 1.48–1.55
1.162.00
化学体系Solvent UV-curable hybrid
固化类型UV
产品系列KM-001–040

规格

功能

AntifoulingHard coatingUV protection

兼容基材

PETPCPMMA

加工方法

SPINDIPROLLGRAVURE

折射率范围

1.48–1.55
1.162.00
属性值
产品代码KM-027
化学体系Solvent UV-curable hybrid
折射率范围1.48–1.55
固化类型UV
PFAS状态无PFAS版本可用 · fluorinated version available on request
功能Antifouling, Hard coating, UV protection
兼容基材PET, PC, PMMA
加工SPIN, DIP, ROLL, GRAVURE
产品系列KM-001–040
批次规模从40 kg样品到量产规模
保质期6个月(未开封)
质量ISO 9001:2015认证。过滤至0.8 µm。每批次最多10个CTQ参数。

申请样品

从40 kg样品批次开始提供。每批次0.8 μm过滤,最多10个CTQ参数测试。

联系我们