KM-004无PFAS版本可用
NIR Absorbing
Near-infrared absorbing coating based on ATO nanoparticle dispersion. Blocks NIR radiation (800–2500 nm) while maintaining high visible light transmission. Designed for automotive glazing and solar heat control applications where reducing cabin temperature and AC load is critical.
规格
功能
NIR absorbing
兼容基材
GlassPET
加工方法
SPINDIPSPRAY
折射率范围
0.00–0.00
1.162.00
| 属性 | 值 |
|---|---|
| 产品代码 | KM-004 |
| 化学体系 | Solvent sol-gel |
| 折射率范围 | 0.00–0.00 |
| 固化类型 | Thermal |
| PFAS状态 | 无PFAS版本可用 |
| 功能 | NIR absorbing |
| 兼容基材 | Glass, PET |
| 加工 | SPIN, DIP, SPRAY |
| 产品系列 | KM-001–040 |
| 批次规模 | 从40 kg样品到量产规模 |
| 保质期 | 6个月(未开封) |
| 质量 | ISO 9001:2015认证。过滤至0.8 µm。每批次最多10个CTQ参数。 |
相关案例
Automotive Thermal<0.3%Haze (automotive grade)ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partnerAutomotive Thermal−9°CCabin temperature reductionCabin temperature reduced by 9°C with ATO glazing integrationAutomotive Thermal+16 kmRange extension (premium segment)16 km additional EV range through solar heat control glazing
申请样品
从40 kg样品批次开始提供。每批次0.8 μm过滤,最多10个CTQ参数测试。