Solar & Energy

3.9% transmission gain on photovoltaic cover glass with thermal-curable LRI

A leading solar module integrator

核心指标

+3.9%Transmission gain
93.8%Coated transmission
630°CTempering survived
0.34%Haze

01

挑战

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

我们的方法

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

成果

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

为什么选择Kriya

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

核心指标

+3.9%Transmission gain
93.8%Coated transmission
630°CTempering survived
0.34%Haze

使用产品