所有案例研究
Architectural Glass

LRI coating survives 630°C tempering, delivers 2.5–4.5× light guiding gain

A European glass industry leader

核心指标

4.5×Luminance improvement
+3.9%Transmission gain
630°CTempering survived
0.34%Haze (C-illuminant)

01

挑战

The glass manufacturer needed an LRI coating at RI 1.37 that could survive furnace tempering (250 seconds at 630°C with rapid cooling) for use in architectural and automotive light-guiding glass. No existing LRI coating on the market was known to withstand this thermal process.

02

我们的方法

Kriya developed both UV-curable and thermal-curable LRI variants at RI 1.37. Testing included direct glass coating with low-E film, PET substrate variants, and tempering survival validation. The thermal-curable variant (095-105-C high-temperature variant) was optimised for the customer’s high-temperature process.

03

成果

The thermal-curable LRI achieved 93.8% transmission (3.9% gain over uncoated substrate) with 0.34% haze. The coating survived full furnace tempering at 630°C with no visible deterioration. Light-guiding tests confirmed 2.5–4.5× luminance improvement versus uncoated glass, comparable to LRI-on-PET performance.

为什么选择Kriya

Kriya is the only supplier offering PFAS-free overcoatable LRI that survives glass tempering temperatures, enabling direct coating of architectural and automotive glass without lamination.

核心指标

4.5×Luminance improvement
+3.9%Transmission gain
630°CTempering survived
0.34%Haze (C-illuminant)

使用产品

讨论类似应用

我们的技术团队可以帮助您评估该方法是否适用于您的特定需求。