Swanepoel 포락선 분석기
How do I extract refractive index and thickness from a transmission spectrum?
코팅 필름 투과 스펙트럼과 기판 단독 기준 스펙트럼으로부터 굴절률 n(λ), 소광 계수 k(λ), 물리적 두께 d를 추출합니다. 다공성 실리카 LRI 코팅을 위해 자체 개발한 폐쇄형 저굴절률 (n < s) 분기를 포함합니다.
How it works
The Swanepoel envelope method fits two smooth curves to the maxima and minima of a transmission spectrum through a thin film on a transparent substrate. The ratio and separation of the envelopes give the refractive index and the thickness; the absorption coefficient follows from the envelope average. The result depends only on the spectrum and the substrate index.
Worked example
a-Si:H envelope from Swanepoel 1983 Table 1
Transmission envelope → thickness, n(λ) via Swanepoel 1983.
Validation method, references and test-case results: /validation#swanepoel