How much group delay dispersion does this stack add?
다층 코팅의 스펙트럼 위상, 군지연 및 군지연 분산. 초단 펄스 거울 및 레이저용 광대역 AR 코팅에 유용합니다.
How it works
A multilayer stack adds a wavelength-dependent reflection phase on top of its amplitude response. The second derivative of that phase with respect to angular frequency is the group delay dispersion, which stretches a short pulse in time. The transfer-matrix method gives the phase directly from the stack definition.
Worked example
4-layer TiO₂ / SiO₂ chirped-mirror reference stack
GDD computed via d(GD)/dω with Macleod sign convention; parity with the TS↔Python reference under tests/.