How does nanoparticle loading change the refractive index of a coating?

제1원리에서 저굴절률 코팅을 설계합니다: 중공 나노입자 기하학(쉘 두께, 직경, 충전 밀도)이 2단계 유효매질 이론을 통해 유효 굴절률을 결정합니다.

How it works

Adding nanoparticles to a polymer host shifts the effective refractive index of the mixture toward the index of the particles. Effective-medium theories (Maxwell-Garnett at low fractions, Bruggeman at higher) relate the loading, host and particle indices to the mixture index. Process-side constraints on viscosity and film continuity bound the practical loading range.

Worked example

Hollow silica 60 nm, shell 8 nm, 55 vol % in binder 1.49

Hollow-silica particles in a binder; Maxwell-Garnett for both the particle and film mixing steps.

Validation method, references and test-case results: /validation#lri-particle