핫/콜드 미러 설계기

How do I design a stack that reflects one band and transmits another?

선택된 IR 또는 가시 컷오프에 대해 4분의 1 파장 HRI/LRI 다이크로익 스택을 설계합니다.

How it works

A dichroic mirror alternates high- and low-index quarter-wave layers tuned to a stopband centred on the reflection target. The stopband width scales with the index contrast between the two materials; the bandpass region on the opposite side of the design wavelength is where the mirror transmits. The transfer-matrix method predicts the full spectrum from the chosen layer set.

Worked example

Hot mirror edge filter, HRI 1.95 / LRI 1.25 on BK7, 700 nm cutoff

Edge-aligned quarter-wave stack; exact pair count from air|(HL)^N|ns admittance.

Validation method, references and test-case results: /validation#hot-cold-mirror

Request accessOpen the interactive tool