CTE 불일치 휨 변형

How large are the thermal-cycling stresses between these two layers?

코팅과 기판을 함께 경화·냉각할 때 발생하는 열팽창 불일치 응력, 기판 곡률, 엣지 새그를 예측합니다. 리소그래피·픽앤플레이스·핸들링 임계값에 대한 경고를 제공합니다.

How it works

A thin coating bonded to a substrate experiences in-plane strain when the two materials have different coefficients of thermal expansion and the stack is heated or cooled. For a thin film on a thick substrate, Stoney's approximation relates the induced stress to the differential strain, the film's biaxial modulus and the temperature change. Plasticity, cracking and delamination follow once the stress exceeds the film's fracture or adhesion strength.

Worked example

PC 1 mm substrate, ΔT 60 K

CTE mismatch × ΔT → biaxial film stress and substrate warpage via Stoney.

Validation method, references and test-case results: /validation#cte-mismatch

Request accessOpen the interactive tool