안티 글레어 광택 & DOI 셀렉터
How do anti-glare roughness and gloss relate for this surface?
60° 목표 광택을 예상 헤이즈, 선명도, DOI를 갖는 AG 등급에 매핑합니다.
How it works
An anti-glare surface scatters a fraction of incident light into angles away from the specular direction, lowering specular gloss and reducing mirror-sharp reflections. The scattered fraction scales with the surface roughness relative to the wavelength. The perceived image clarity trades off against the glare reduction.
Worked example
60° gloss 70 + DOI 85 → Kriya AG-7085
ASTM D523 + D5767 grid lookup.
Validation method, references and test-case results: /validation#ag-gloss-doi