모든 도입 사례
디스플레이

ULR 코팅, 편광 필름에서 0.41% 헤이즈 달성 (기존 0.68% 대비)

아시아 주요 디스플레이 필름 제조업체

핵심 지표

0.41%헤이즈 (기존 0.68% 대비)
4H연필 경도 (3H 대비)
97.0%투과율 (C광원)
0%기재 컬

01

과제

The display film producer needed an ultra-low-reflection coating on TAC polariser film that could match or exceed the performance of the incumbent Japanese supplier. The existing solution suffered from strong substrate curl and higher haze, impacting yield and optical quality in large-format TV panel production.

02

접근 방법

Kriya developed a 4-layer ULR stack (HC + HRI + HRI + ARAF) on 60 µm TAC substrate. Hand-coated prototypes were benchmarked head-to-head against machine-coated competitor samples. Optical modelling confirmed reflection below 0.2% across the 450–650 nm visible band, and formulation was iterated through three versions to optimise haze-reflection balance.

03

성과

Kriya ULR achieved 0.41% haze (C-illuminant) versus 0.68% for the competitor—a 40% haze reduction. Pencil hardness reached 4H (vs 3H), transmission matched at 97.0%, and the Kriya coating eliminated substrate curl entirely. Steel wool abrasion at 10 rubs showed no scratches versus visible scratches on the competitor film.

Kriya를 선택하는 이유

Kriya is the only PFAS-free supplier with overcoatable LRI down to RI 1.16, enabling the full multi-layer AR stack from a single vendor with no curl and superior mechanical durability.

핵심 지표

0.41%헤이즈 (기존 0.68% 대비)
4H연필 경도 (3H 대비)
97.0%투과율 (C광원)
0%기재 컬

사용 제품

관련 응용 분야

Displays →

유사한 응용 상담

기술팀이 귀하의 요구사항에 이 접근 방법이 적용 가능한지 평가해 드리겠습니다.

대화 시작