모든 도입 사례
태양광 및 에너지

열경화 LRI로 태양전지 커버 유리 투과율 3.9% 향상

주요 태양광 모듈 통합업체

핵심 지표

+3.9%투과율 향상
93.8%코팅 후 투과율
630°C강화 처리 통과
0.34%헤이즈

01

과제

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

접근 방법

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

성과

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

Kriya를 선택하는 이유

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

핵심 지표

+3.9%투과율 향상
93.8%코팅 후 투과율
630°C강화 처리 통과
0.34%헤이즈

사용 제품