과제

The OEM required a multi-functional coating for foldable displays that combined hard coating, antistatic, and antifouling properties in a single layer. The coating had to survive 200,000 fold cycles at 1.5R radius without cracking or loss of surface properties, and had to be PFAS-free to meet upcoming regulatory requirements.

02

접근 방법

Kriya formulated a UV-curable multi-functional coating (35 wt% solids) on 75 µm PET, combining hard coating, antistatic (10⁹ Ω/sq), and antifouling (WCA 110°) in a single layer. The coating was validated through exhaustive QC including 2,000-cycle steel wool abrasion, ballpoint pen drop tests, and permanent marker wipe-off testing.

03

성과

The coating passed all qualification criteria: pencil hardness 3H, surface resistivity 8.0×10⁹ Ω/sq, WCA retained above 95° after 2,000 steel wool cycles at 1 kg/cm², and permanent marker wipe-off confirmed. The coating passes 200,000 fold cycles at 1.5R, compatible with R2R processing for volume production.

Kriya를 선택하는 이유

Kriya delivered three functions in one PFAS-free layer, eliminating separate coating steps and reducing both processing cost and regulatory risk for the OEM’s foldable product line.

핵심 지표

200k폴딩 사이클 통과
3HPencil hardness
2,000x스틸울 사이클 통과
>95°마모 후 WCA

사용 제품

관련 응용 분야

Displays — Foldable →

유사한 응용 상담

기술팀이 귀하의 요구사항에 이 접근 방법이 적용 가능한지 평가해 드리겠습니다.

대화 시작