모든 도입 사례
디스플레이 — 폴더블

PFAS-free 플렉서블 AR, WCA >100° 달성, PFAS보다 우수한 유지력

한국 주요 디스플레이 Tier-1 업체

핵심 지표

>100°수접촉각 (PFAS-free)
SuperiorPFAS 대비 WCA 유지력
Pass방오 내구성
R2R양산 호환

01

과제

With PFAS regulation tightening globally, the display OEM needed a PFAS-free anti-reflective and anti-fouling solution for foldable displays that could match or exceed the surface property retention of incumbent PFAS-based coatings under repeated mechanical stress.

02

접근 방법

Kriya’s PFAS-free ARAF technology, based on functionalised HSiO₂ nanoparticles, was tested against PFAS-based references for water contact angle, anti-smudge durability, and retention after steel wool abrasion cycles. The formulation was designed for UV cure compatibility with R2R processing.

03

성과

The PFAS-free coating achieved WCA above 100° with superior retention versus PFAS-based alternatives after repeated abrasion. Anti-smudge properties (fingerprint resistance and marker wipe-off) were maintained across the full test protocol. The coating is R2R-compatible for volume production.

Kriya를 선택하는 이유

Kriya provides a complete PFAS-free alternative that actually outperforms PFAS on durability retention, eliminating regulatory risk while improving product performance.

핵심 지표

>100°수접촉각 (PFAS-free)
SuperiorPFAS 대비 WCA 유지력
Pass방오 내구성
R2R양산 호환

사용 제품

관련 응용 분야

Displays — Foldable →