모든 도입 사례
자동차 열관리

태양열 제어 글레이징으로 EV 주행 거리 16km 연장

EV 차량 모델 대상 연구 수행

핵심 지표

+16 km주행 거리 연장 (프리미엄 세그먼트)
€325차량당 배터리 절감
35%에어컨 전력 절감
100%5G/RF/LiDAR 투과

01

과제

The EV manufacturer needed to extend vehicle range without increasing battery size, which adds weight and cost. AC power consumption in warm climates was identified as a significant parasitic load, particularly during the regulatory shift toward stricter EU CO₂ targets that penalise each g/km above target at €95 per vehicle.

02

접근 방법

Kriya’s ATO solar heat control glazing was modelled for the premium EV segment (85.6 kWh average battery, 442 km WLTP range). The integration blocks 250 W/m² of NIR solar radiation while remaining fully transparent to 5G, RF, and LiDAR signals—a critical requirement that ITO-based alternatives cannot meet.

03

성과

The analysis showed up to 16 km range extension, 8.5 kg battery saving equivalent to approximately €325 per vehicle, and 35% AC power reduction. For the compact segment (39.3 kWh, 227 km), the extension was 7 km with 4.6 kg battery saving worth approximately €159.

Kriya를 선택하는 이유

Unlike ITO alternatives, Kriya ATO does not block RF signals, making it the only viable solar heat control solution for connected and autonomous vehicles.

핵심 지표

+16 km주행 거리 연장 (프리미엄 세그먼트)
€325차량당 배터리 절감
35%에어컨 전력 절감
100%5G/RF/LiDAR 투과

사용 제품

관련 응용 분야

Automotive Thermal →

유사한 응용 상담

기술팀이 귀하의 요구사항에 이 접근 방법이 적용 가능한지 평가해 드리겠습니다.

대화 시작