다층 AR 스택에서 광대역 반사율 0.15% 이하 달성

주요 Tier-1 디스플레이 광학 필름 제조업체

핵심 지표

<0.15%잔류 반사율
+3.3%투과율 향상 (PET)
100%모든 기재에서의 밀착성
4검증된 기재 수

01

과제

The consumer-electronics company required a broadband anti-reflective coating stack achieving residual reflectance below 0.15% across the visible spectrum. The solution had to be PFAS-free and compatible with their existing substrate portfolio (PET, PC, PMMA, TAC).

02

접근 방법

Kriya designed a multi-layer AR stack utilising the full RI platform from 1.16 to 1.95. The stack was optimised through optical modelling and validated on four substrates, measuring transmission gain, haze, reflection, pencil hardness, and adhesion per ISO and ASTM standards.

03

성과

Broadband residual reflectance below 0.15% was achieved on the multi-layer stack. Transmission gains ranged from 2.2% (PMMA) to 3.3% (PET), with 100% adhesion on all substrates. Pencil hardness varied by substrate from HB (PC) to 4H (PMMA). All formulations were PFAS-free.

Kriya를 선택하는 이유

Kriya offers the widest PFAS-free RI range (1.16–2.00) from a single supplier, enabling complete multi-layer AR stacks without sourcing from multiple vendors.

핵심 지표

<0.15%잔류 반사율
+3.3%투과율 향상 (PET)
100%모든 기재에서의 밀착성
4검증된 기재 수