모든 도입 사례
자동차 열관리

PVB 내 ATO, 2,000시간 가속 내후성 시험 통과

Tier-1 PVB 중간막 제조업체

핵심 지표

2,000 hr가속 내후성 시험 통과
<0.3%헤이즈 유지
PassNIR 차단 유지
0유의미한 열화

01

과제

Before committing to production integration, the Tier-1 PVB interlayer manufacturer required long-term durability validation of ATO nanoparticles in PVB under accelerated weathering conditions. Automotive glazing must maintain optical and thermal performance for the lifetime of the vehicle.

02

접근 방법

Kriya ATO in PVB samples were subjected to 2,000-hour accelerated weathering per automotive industry standards. Optical properties (transmission, haze, SHGC) and mechanical integrity were measured at intervals throughout the test programme.

03

성과

All samples passed the full 2,000-hour accelerated weathering protocol with no significant degradation of optical or thermal properties. Haze remained below 0.3%, and NIR blocking performance was maintained. The results validated ATO-PVB as production-ready for automotive glazing.

Kriya를 선택하는 이유

Kriya’s bottom-up synthesised ATO nanoparticles are inherently more stable than ball-milled alternatives because the controlled synthesis produces uniform particle size with consistent surface chemistry.

핵심 지표

2,000 hr가속 내후성 시험 통과
<0.3%헤이즈 유지
PassNIR 차단 유지
0유의미한 열화

사용 제품