과제

The Tier-1 PVB interlayer partner needed an ATO dispersion for solar heat control interlayer film that could achieve automotive-grade haze (<0.5%) when laminated with green glass. Previous ATO suppliers using top-down ball-milling produced dispersions with haze exceeding 1.7%, far above automotive requirements.

02

접근 방법

Kriya provided four ATO dispersion variants at 8.3 wt% concentration for evaluation. The partner laminated samples with 2.0 mm green glass and measured optical properties including visible light transmission, total solar transmittance, and haze according to their internal automotive qualification protocol.

03

성과

The optimised variant achieved 0.2% haze at 0.10 wt% and 0.3% haze at 0.20 wt% in PVB—the only samples passing the partner’s automotive haze threshold. Visible light transmission ranged from 71–75%, and total solar transmittance from 58–61%. The partner concluded the technology had "great potential."

Kriya를 선택하는 이유

Kriya’s proprietary bottom-up ATO synthesis produces nanoparticles with fundamentally lower scattering than ball-milled alternatives, achieving 5× better effectiveness at equal SHGC versus the leading competitor.