Calculadora de contracción por curado

How much does this resin shrink on cure?

Estima el espesor de película seca, la pérdida volumétrica y el factor de aumento de densidad debidos a la contracción por curado de la familia química elegida.

How it works

A curing resin shrinks as its monomers polymerise into a denser network. The shrinkage fraction depends on the monomer chemistry and the achieved degree of cure. The induced residual stress adds to any thermal-mismatch stress in the finished coating.

Worked example

UV acrylate, 5 % volume shrinkage, 10 µm wet film

Constrained-film cure shrinkage: all volume loss projected into thickness.

Validation method, references and test-case results: /validation#cure-shrinkage

Request accessOpen the interactive tool