容差蒙特卡罗
What is the yield of this stack under production variation?
通过对数千个样本模拟各层厚度及折射率的偏差,评估镀膜堆栈设计在实际生产容差下的性能表现。
How it works
Manufacturing tolerance analysis samples the stack's forward model many times with layer thickness and index perturbed by their process standard deviations. The resulting distribution of the specified metric (band-averaged reflectance, colour shift, et cetera) gives the percentile bands and the yield at a given acceptance limit. The sensitivity of the yield to each parameter follows from the partial derivatives of the metric at the nominal design.
Worked example
Kriya 4-layer broadband, ±3 nm / ±0.01 n, 500 runs
Monte Carlo over thickness + n tolerances; σ(R) and yield-at-spec.
Validation method, references and test-case results: /validation#tolerance-mc