How do I extract refractive index and thickness from a transmission spectrum?
从镀膜薄膜透射光谱及裸基底参考光谱中提取折射率 n(λ)、消光系数 k(λ) 与物理厚度 d,包含内部推导的低折射率(n < s)分支解析解,适用于多孔二氧化硅 LRI 涂层。
How it works
The Swanepoel envelope method fits two smooth curves to the maxima and minima of a transmission spectrum through a thin film on a transparent substrate. The ratio and separation of the envelopes give the refractive index and the thickness; the absorption coefficient follows from the envelope average. The result depends only on the spectrum and the substrate index.
Worked example
a-Si:H envelope from Swanepoel 1983 Table 1
Transmission envelope → thickness, n(λ) via Swanepoel 1983.
Validation method, references and test-case results: /validation#swanepoel