LRI 颗粒工程模型

How does nanoparticle loading change the refractive index of a coating?

从第一原理出发设计低折射率涂层:中空纳米颗粒的几何参数(壳厚、直径、堆积密度)通过两级有效介质理论决定有效折射率。

How it works

Adding nanoparticles to a polymer host shifts the effective refractive index of the mixture toward the index of the particles. Effective-medium theories (Maxwell-Garnett at low fractions, Bruggeman at higher) relate the loading, host and particle indices to the mixture index. Process-side constraints on viscosity and film continuity bound the practical loading range.

Worked example

Hollow silica 60 nm, shell 8 nm, 55 vol % in binder 1.49

Hollow-silica particles in a binder; Maxwell-Garnett for both the particle and film mixing steps.

Validation method, references and test-case results: /validation#lri-particle

Request accessOpen the interactive tool