Ghost Lab

What does the eye actually see reflected off a coated surface?

还原眼睛所见。在镀膜表面上渲染点亮场景的鬼像反射,并从任意角度观察。亮度与色彩均来自与 TMM Simulator 相同的传递矩阵核。

How it works

A coated surface reflects a fraction of every wavelength in the ambient scene, weighted by the coating's spectral and angular response. Rendering that physical reflection requires combining a scene radiance distribution with the surface reflectance spectrum at each pixel and applying a camera tone curve. The transfer-matrix method supplies the reflectance input for isotropic multilayer stacks.

Worked example

Bare glass vs single-layer n 1.22 vs 4-layer, D65, 30°

Shows the ghost ladder — 4.3 % → 0.01 % → 0.3 % photopic R.

Validation method, references and test-case results: /validation#ghost-lab

Request accessOpen the interactive tool