CTE 失配翘曲

How large are the thermal-cycling stresses between these two layers?

预测涂层与基板共同固化冷却时的热膨胀失配应力、基板曲率及边缘矢高,并标记光刻 / 贴片 / 操作工艺阈值。

How it works

A thin coating bonded to a substrate experiences in-plane strain when the two materials have different coefficients of thermal expansion and the stack is heated or cooled. For a thin film on a thick substrate, Stoney's approximation relates the induced stress to the differential strain, the film's biaxial modulus and the temperature change. Plasticity, cracking and delamination follow once the stress exceeds the film's fracture or adhesion strength.

Worked example

PC 1 mm substrate, ΔT 60 K

CTE mismatch × ΔT → biaxial film stress and substrate warpage via Stoney.

Validation method, references and test-case results: /validation#cte-mismatch