How much ambient light degrades the contrast of a display?
在有环境光照的房间内,显示屏的实际对比度——计入发光体上方所有反射面的影响,而不仅限于最前端的表面。
How it works
Display contrast under ambient light is the ratio of light emitted from a bright pixel plus reflected ambient to light emitted from a dark pixel plus reflected ambient. Surface and internal reflectance together with ambient illuminance set the reflected term. Anti-reflection and anti-glare layers reduce both.
Worked example
800 nit display, 10 000 lux ambient, two-surface stack
Ambient contrast ratio from veiling luminance; adjust surface R to see the delta.