所有产品
KM-404无PFAS版本可用
Add NIR to External Material
ATO nanoparticle dispersion additive that can be incorporated into third-party materials to add NIR absorption. Bottom-up synthesised with haze <0.3%. Compatible with PVB, PU, and other host matrices for automotive and architectural glazing.
规格
功能
NIR absorbing
兼容基材
PVBPUGlass
加工方法
SPRAYDIP
折射率范围
0.00–0.00
1.162.00
| 属性 | 值 |
|---|---|
| 产品代码 | KM-404 |
| 化学体系 | Solvent sol-gel |
| 折射率范围 | 0.00–0.00 |
| 固化类型 | Thermal |
| PFAS状态 | 无PFAS版本可用 |
| 功能 | NIR absorbing |
| 兼容基材 | PVB, PU, Glass |
| 加工 | SPRAY, DIP |
| 产品系列 | KM-401–409 |
| 批次规模 | 从40 kg样品到量产规模 |
| 保质期 | 6个月(未开封) |
| 质量 | ISO 9001:2015认证。过滤至0.8 µm。每批次最多10个CTQ参数。 |
相关案例
Automotive Thermal<0.3%Haze (automotive grade)ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partnerAutomotive Thermal−9°CCabin temperature reductionCabin temperature reduced by 9°C with ATO glazing integrationAutomotive Thermal+16 kmRange extension (premium segment)16 km additional EV range through solar heat control glazing
申请样品
从40 kg样品批次开始提供。每批次0.8 μm过滤,最多10个CTQ参数测试。