所有产品
KM-006无PFAS版本可用
High Refractive Index
High refractive index coating tuneable from RI 1.65 to 2.00 via sol-gel nanoparticle chemistry. Achieves pencil hardness up to 8H on glass substrates. Essential building block for multi-layer AR stacks, waveguide cores, and index-matching applications.
规格
功能
High RI
兼容基材
GlassPETPCPMMA
加工方法
SPINDIPROLLSPRAY
折射率范围
1.65–2.00
1.162.00
| 属性 | 值 |
|---|---|
| 产品代码 | KM-006 |
| 化学体系 | Solvent sol-gel |
| 折射率范围 | 1.65–2.00 |
| 固化类型 | Thermal |
| PFAS状态 | 无PFAS版本可用 |
| 功能 | High RI |
| 兼容基材 | Glass, PET, PC, PMMA |
| 加工 | SPIN, DIP, ROLL, SPRAY |
| 产品系列 | KM-001–040 |
| 批次规模 | 从40 kg样品到量产规模 |
| 保质期 | 6个月(未开封) |
| 质量 | ISO 9001:2015认证。过滤至0.8 µm。每批次最多10个CTQ参数。 |
相关案例
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmOptical Components8HPencil hardness at RI 1.85Thermal HRI coating reaches RI > 1.8 and 8H pencil hardness on specialty glassDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stack
申请样品
从40 kg样品批次开始提供。每批次0.8 μm过滤,最多10个CTQ参数测试。