所有产品
KM-003无PFAS版本可用
Antifouling
Antifouling coating available as a PFAS-free variant, with water contact angle exceeding 100°. Resists fingerprints and smudges while maintaining optical clarity. Functionalised HSiO₂ nanoparticles provide durable easy-clean properties without perfluorinated chemistry.
规格
功能
AntifoulingAnti-smudge
兼容基材
PETPCPMMATACGlass
加工方法
SPINDIPROLLGRAVURE
折射率范围
1.40–1.50
1.162.00
| 属性 | 值 |
|---|---|
| 产品代码 | KM-003 |
| 化学体系 | Solvent UV-curable hybrid |
| 折射率范围 | 1.40–1.50 |
| 固化类型 | UV |
| PFAS状态 | 无PFAS版本可用 · fluorinated version available on request |
| 功能 | Antifouling, Anti-smudge |
| 兼容基材 | PET, PC, PMMA, TAC, Glass |
| 加工 | SPIN, DIP, ROLL, GRAVURE |
| 产品系列 | KM-001–040 |
| 批次规模 | 从40 kg样品到量产规模 |
| 保质期 | 6个月(未开封) |
| 质量 | ISO 9001:2015认证。过滤至0.8 µm。每批次最多10个CTQ参数。 |
相关案例
Displays — Foldable200kFold cycles passedSingle-layer hardcoat passes 200,000 fold cycles with PFAS-free anti-smudgeDisplays — ULR0.3×Reflection vs referenceARAF nanoparticle composition achieves 0.3× reference reflection levelDisplays — Foldable>100°Water contact angle (PFAS-free)PFAS-free flexible AR achieves WCA >100° with better retention than PFAS
申请样品
从40 kg样品批次开始提供。每批次0.8 μm过滤,最多10个CTQ参数测试。