所有案例研究
Automotive Thermal

ATO in PVB passes 2,000-hour accelerated weathering test

A Tier-1 PVB interlayer manufacturer

核心指标

2,000 hrAccelerated weathering passed
<0.3%Haze maintained
PassNIR blocking retained
0Significant degradation

01

挑战

Before committing to production integration, the Tier-1 PVB interlayer manufacturer required long-term durability validation of ATO nanoparticles in PVB under accelerated weathering conditions. Automotive glazing must maintain optical and thermal performance for the lifetime of the vehicle.

02

我们的方法

Kriya ATO in PVB samples were subjected to 2,000-hour accelerated weathering per automotive industry standards. Optical properties (transmission, haze, SHGC) and mechanical integrity were measured at intervals throughout the test programme.

03

成果

All samples passed the full 2,000-hour accelerated weathering protocol with no significant degradation of optical or thermal properties. Haze remained below 0.3%, and NIR blocking performance was maintained. The results validated ATO-PVB as production-ready for automotive glazing.

为什么选择Kriya

Kriya’s bottom-up synthesised ATO nanoparticles are inherently more stable than ball-milled alternatives because the controlled synthesis produces uniform particle size with consistent surface chemistry.

核心指标

2,000 hrAccelerated weathering passed
<0.3%Haze maintained
PassNIR blocking retained
0Significant degradation

使用产品

讨论类似应用

我们的技术团队可以帮助您评估该方法是否适用于您的特定需求。