所有案例研究
Automotive Thermal

ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partner

A Tier-1 PVB interlayer manufacturer

核心指标

<0.3%Haze (automotive grade)
5×More effective vs competitor at equal SHGC
~60%Cost vs ITO
75%Visible light transmission

01

挑战

The Tier-1 PVB interlayer partner needed an ATO dispersion for solar heat control interlayer film that could achieve automotive-grade haze (<0.5%) when laminated with green glass. Previous ATO suppliers using top-down ball-milling produced dispersions with haze exceeding 1.7%, far above automotive requirements.

02

我们的方法

Kriya provided four ATO dispersion variants at 8.3 wt% concentration for evaluation. The partner laminated samples with 2.0 mm green glass and measured optical properties including visible light transmission, total solar transmittance, and haze according to their internal automotive qualification protocol.

03

成果

The optimised variant achieved 0.2% haze at 0.10 wt% and 0.3% haze at 0.20 wt% in PVB—the only samples passing the partner’s automotive haze threshold. Visible light transmission ranged from 71–75%, and total solar transmittance from 58–61%. The partner concluded the technology had "great potential."

为什么选择Kriya

Kriya’s proprietary bottom-up ATO synthesis produces nanoparticles with fundamentally lower scattering than ball-milled alternatives, achieving 5× better effectiveness at equal SHGC versus the leading competitor.

核心指标

<0.3%Haze (automotive grade)
5×More effective vs competitor at equal SHGC
~60%Cost vs ITO
75%Visible light transmission

使用产品

讨论类似应用

我们的技术团队可以帮助您评估该方法是否适用于您的特定需求。