Modelo de ingeniería de partículas LRI
How does nanoparticle loading change the refractive index of a coating?
Diseñe recubrimientos de bajo índice de refracción desde primeros principios: la geometría de nanopartículas huecas (espesor de cáscara, diámetro, densidad de empaque) determina el RI efectivo mediante teoría de medio efectivo de dos niveles.
How it works
Adding nanoparticles to a polymer host shifts the effective refractive index of the mixture toward the index of the particles. Effective-medium theories (Maxwell-Garnett at low fractions, Bruggeman at higher) relate the loading, host and particle indices to the mixture index. Process-side constraints on viscosity and film continuity bound the practical loading range.
Worked example
Hollow silica 60 nm, shell 8 nm, 55 vol % in binder 1.49
Hollow-silica particles in a binder; Maxwell-Garnett for both the particle and film mixing steps.
Validation method, references and test-case results: /validation#lri-particle