Calculadora de transmisión de ventana LIDAR
How much signal does the cover window lose for a 905 nm or 1550 nm LiDAR?
Calcula la ganancia de transmisión de ida y vuelta al añadir un recubrimiento AR Kriya a una ventana de cubierta LIDAR a 905, 940 o 1550 nm.
How it works
A LiDAR cover window sees the emission pulse twice — once outbound, once on the return. Each pass is attenuated by the coated window's transmittance at the laser wavelength, so the signal returned to the detector scales as the square of the single-pass transmittance. A narrow-band anti-reflection coating recovers most of the loss at the design wavelength.
Worked example
Lossless incoherent slab, n 1.52: R_total = 2R / (1 + R)
Inputs: nSlab = 1.52
Result: 8.168 %
Reference: Born & Wolf §1.6.3 — thick-slab incoherent sum
Computed by this tool's kernel at build (commit dae6663).