How large are the thermal-cycling stresses between these two layers?

Predice la tensión por desajuste de expansión térmica, la curvatura del sustrato y la flecha en el borde cuando un recubrimiento y su sustrato se curan y enfrían juntos. Señala umbrales de litografía, colocación y manipulación.

How it works

A thin coating bonded to a substrate experiences in-plane strain when the two materials have different coefficients of thermal expansion and the stack is heated or cooled. For a thin film on a thick substrate, Stoney's approximation relates the induced stress to the differential strain, the film's biaxial modulus and the temperature change. Plasticity, cracking and delamination follow once the stress exceeds the film's fracture or adhesion strength.

Worked example

PC 1 mm substrate, ΔT 60 K

CTE mismatch × ΔT → biaxial film stress and substrate warpage via Stoney.

Validation method, references and test-case results: /validation#cte-mismatch