Desplazamiento de color / Índice arcoíris
How much does the reflected colour change with viewing angle?
Cuantifica el desplazamiento angular de color («arcoíris») de un stack multicapa visto por un observador humano, mediante colorimetría CIE.
How it works
Reflected spectra from thin films depend on the optical path length through each layer, which lengthens with increasing angle of incidence. Integrating the angle-dependent reflectance against a reference illuminant gives the reflected colour; the perceptual shift between two angles is quantified by the CIE ΔE* colour-difference metric in a uniform colour space such as CIELAB.
Worked example
CIEDE2000 Sharma pair 1
Inputs: lab1 = {"L":50,"a":2.6772,"b":-79.7751}, lab2 = {"L":50,"a":0,"b":-82.7485}
Result: 2.042 ΔE₀₀
Reference: Sharma, Wu & Dalal 2005 Color Res. Appl. 30, 21
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#colour-shift