Todos los casos de estudio
Componentes ópticos

El recubrimiento HRI térmico alcanza RI > 1,8 y dureza de lápiz 8H en vidrio especial

Un fabricante de vidrio especial

Indicadores clave

8HDureza de lápiz a RI 1,85
0.49%Menor turbidez alcanzada
100%Adherencia (ASTM D3359)
130°CTemperatura mínima de curado

01

El desafío

The glass manufacturer needed a high refractive index coating on display glass (0.7 mm) that could achieve RI 1.85 with maximum hardness. Existing HRI coatings from other suppliers could not reach 8H pencil hardness at these RI levels, and lower cure temperatures were desired to reduce energy costs.

02

Nuestro enfoque

Kriya developed three thermal-curable HRI formulation variants (V1, V2, V3), testing cure temperatures from 130°C to 200°C. Formulation optimisation focused on reducing haze through organic compound reduction (V2, V3) while maintaining RI and hardness targets. Low-outgassing variants were developed in response to customer requirements.

03

El resultado

V1 achieved RI 1.85 and 8H pencil hardness across all cure temperatures (130–200°C). V2 delivered the lowest haze: 0.49% at 200°C cure. All variants achieved 100% adhesion (ASTM D3359). Higher cure temperatures reduced haze significantly, with the majority of improvement occurring at 160°C.

Por qué Kriya

Kriya’s sol-gel chemistry uniquely enables 8H pencil hardness at RI 1.85 via thermal cure alone, with tuneable cure temperatures and low-outgassing options that competitors cannot match.

Indicadores clave

8HDureza de lápiz a RI 1,85
0.49%Menor turbidez alcanzada
100%Adherencia (ASTM D3359)
130°CTemperatura mínima de curado

Productos utilizados

Aplicación relacionada

Optical Components →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación