Todos los casos de estudio
Solar y energía

Ganancia de transmisión del 3,9 % en vidrio de cubierta fotovoltaica con LRI termocurable

Un integrador líder de módulos solares

Indicadores clave

+3.9%Ganancia de transmisión
93.8%Transmisión con recubrimiento
630°CTemplado superado
0.34%Turbidez

01

El desafío

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

Nuestro enfoque

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

El resultado

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

Por qué Kriya

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

Indicadores clave

+3.9%Ganancia de transmisión
93.8%Transmisión con recubrimiento
630°CTemplado superado
0.34%Turbidez

Productos utilizados

Aplicación relacionada

Solar & Energy →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación