Todos los casos de estudio
Vidrio arquitectónico

El recubrimiento LRI resiste el templado a 630 °C y ofrece una ganancia de guía de luz de 2,5 a 4,5 veces

Un líder europeo de la industria del vidrio

Indicadores clave

4.5×Mejora de luminancia
+3.9%Ganancia de transmisión
630°CTemplado superado
0.34%Turbidez (iluminante C)

01

El desafío

The glass manufacturer needed an LRI coating at RI 1.37 that could survive furnace tempering (250 seconds at 630°C with rapid cooling) for use in architectural and automotive light-guiding glass. No existing LRI coating on the market was known to withstand this thermal process.

02

Nuestro enfoque

Kriya developed both UV-curable and thermal-curable LRI variants at RI 1.37. Testing included direct glass coating with low-E film, PET substrate variants, and tempering survival validation. The thermal-curable variant (095-105-C high-temperature variant) was optimised for the customer’s high-temperature process.

03

El resultado

The thermal-curable LRI achieved 93.8% transmission (3.9% gain over uncoated substrate) with 0.34% haze. The coating survived full furnace tempering at 630°C with no visible deterioration. Light-guiding tests confirmed 2.5–4.5× luminance improvement versus uncoated glass, comparable to LRI-on-PET performance.

Por qué Kriya

Kriya is the only supplier offering PFAS-free overcoatable LRI that survives glass tempering temperatures, enabling direct coating of architectural and automotive glass without lamination.

Indicadores clave

4.5×Mejora de luminancia
+3.9%Ganancia de transmisión
630°CTemplado superado
0.34%Turbidez (iluminante C)

Productos utilizados

Aplicación relacionada

Architectural Glass →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación