Todos los casos de estudio
Pantallas — Plegables

Capa dura monocapa supera 200.000 ciclos de plegado con antisuciedad libre de PFAS

Un importante Tier-1 de pantallas coreano

Indicadores clave

200kCiclos de plegado superados
3HPencil hardness
2,000xCiclos de lana de acero superados
>95°WCA tras abrasión

01

El desafío

The OEM required a multi-functional coating for foldable displays that combined hard coating, antistatic, and antifouling properties in a single layer. The coating had to survive 200,000 fold cycles at 1.5R radius without cracking or loss of surface properties, and had to be PFAS-free to meet upcoming regulatory requirements.

02

Nuestro enfoque

Kriya formulated a UV-curable multi-functional coating (35 wt% solids) on 75 µm PET, combining hard coating, antistatic (10⁹ Ω/sq), and antifouling (WCA 110°) in a single layer. The coating was validated through exhaustive QC including 2,000-cycle steel wool abrasion, ballpoint pen drop tests, and permanent marker wipe-off testing.

03

El resultado

The coating passed all qualification criteria: pencil hardness 3H, surface resistivity 8.0×10⁹ Ω/sq, WCA retained above 95° after 2,000 steel wool cycles at 1 kg/cm², and permanent marker wipe-off confirmed. The coating passes 200,000 fold cycles at 1.5R, compatible with R2R processing for volume production.

Por qué Kriya

Kriya delivered three functions in one PFAS-free layer, eliminating separate coating steps and reducing both processing cost and regulatory risk for the OEM’s foldable product line.

Indicadores clave

200kCiclos de plegado superados
3HPencil hardness
2,000xCiclos de lana de acero superados
>95°WCA tras abrasión

Productos utilizados

Aplicación relacionada

Displays — Foldable →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación