AR flexible libre de PFAS alcanza WCA >100° con mejor retención que el PFAS

Un importante Tier-1 de pantallas coreano

Indicadores clave

>100°Ángulo de contacto con agua (libre de PFAS)
SuperiorRetención de WCA frente a PFAS
PassDurabilidad antisuciedad
R2RCompatible con producción

01

El desafío

With PFAS regulation tightening globally, the display OEM needed a PFAS-free anti-reflective and anti-fouling solution for foldable displays that could match or exceed the surface property retention of incumbent PFAS-based coatings under repeated mechanical stress.

02

Nuestro enfoque

Kriya’s PFAS-free ARAF technology, based on functionalised HSiO₂ nanoparticles, was tested against PFAS-based references for water contact angle, anti-smudge durability, and retention after steel wool abrasion cycles. The formulation was designed for UV cure compatibility with R2R processing.

03

El resultado

The PFAS-free coating achieved WCA above 100° with superior retention versus PFAS-based alternatives after repeated abrasion. Anti-smudge properties (fingerprint resistance and marker wipe-off) were maintained across the full test protocol. The coating is R2R-compatible for volume production.

Por qué Kriya

Kriya provides a complete PFAS-free alternative that actually outperforms PFAS on durability retention, eliminating regulatory risk while improving product performance.

Indicadores clave

>100°Ángulo de contacto con agua (libre de PFAS)
SuperiorRetención de WCA frente a PFAS
PassDurabilidad antisuciedad
R2RCompatible con producción

Productos utilizados

Aplicación relacionada

Displays — Foldable →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación