Reflectancia residual de banda ancha inferior al 0,15 % en apilamiento AR multicapa

Un fabricante líder Tier-1 de películas ópticas para pantallas

Indicadores clave

<0.15%Reflectancia residual
+3.3%Ganancia de transmisión (PET)
100%Adherencia en todos los sustratos
4Sustratos validados

01

El desafío

The consumer-electronics company required a broadband anti-reflective coating stack achieving residual reflectance below 0.15% across the visible spectrum. The solution had to be PFAS-free and compatible with their existing substrate portfolio (PET, PC, PMMA, TAC).

02

Nuestro enfoque

Kriya designed a multi-layer AR stack utilising the full RI platform from 1.16 to 1.95. The stack was optimised through optical modelling and validated on four substrates, measuring transmission gain, haze, reflection, pencil hardness, and adhesion per ISO and ASTM standards.

03

El resultado

Broadband residual reflectance below 0.15% was achieved on the multi-layer stack. Transmission gains ranged from 2.2% (PMMA) to 3.3% (PET), with 100% adhesion on all substrates. Pencil hardness varied by substrate from HB (PC) to 4H (PMMA). All formulations were PFAS-free.

Por qué Kriya

Kriya offers the widest PFAS-free RI range (1.16–2.00) from a single supplier, enabling complete multi-layer AR stacks without sourcing from multiple vendors.

Indicadores clave

<0.15%Reflectancia residual
+3.3%Ganancia de transmisión (PET)
100%Adherencia en todos los sustratos
4Sustratos validados

Productos utilizados

Aplicación relacionada

Displays →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación