Safety glasses and visors
Safety glasses and visors are polycarbonate, chosen for impact strength — and polycarbonate is soft and charges easily. The standards allow two optional marks on the lens that buyers look for: resistance to surface damage by fine particles, and resistance to fogging. The first is a hard coat. Dust that clings to a charged lens gets wiped across it, so a hard coat that also bleeds off charge protects itself.
All layers (5)
- Easy-clean topcoat Outer faceK2
- Antistatic hard coat, outer face Mark K: resistance to surface damage by fine particlesK1
- Polycarbonate lens or visor n 1.59
- Hard coat, inner faceK1
- Anti-fog coating, inner face Mark N: resistance to fogging · not Kriya
Working method
Version 1 · first publishedAn antistatic hard coat on both faces and an easy-clean layer outside; the anti-fog layer inside is a different chemistry.
Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.
- Antistatic hard coat on both faces
Pencil hardness 3H+ to 4H on polycarbonate; surface resistance 10⁶–10¹² Ω/sq.
Layers: Antistatic hard coat, outer face · Hard coat, inner face - Easy-clean top layer on the outer face
Water contact angle above 100° without fluorinated chemistry.
Layers: Easy-clean topcoat - Anti-fog layer on the inner face
Not Kriya. The hard coat underneath has to accept it.
Layers: Anti-fog coating, inner face
Public basis
Earlier public documents that describe the same steps.
- US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998: UV-curable transparent coating made antistatic with conductive tin-oxide powder, on substrates such as polycarbonate.
- EP 0 232 033 — Transparent electrically conductive plastic molded articles — 1987: transparent, abrasion-resistant antistatic coat with tin-oxide powder on plastic mouldings.
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993: spin-coated hard coat on plastic lenses, cured by ultraviolet light.
Stays with the device maker
Lens or visor moulding, marking and certification.
A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.
Public references
- BSI white paper: Protective Eyewear suite of standards — BS EN ISO 16321-1, -2 and -3 — EN ISO 16321 replaces EN 166; optional requirements and lens marking
- US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
- EP 0 232 033 — Transparent electrically conductive plastic molded articles — 1987 publication: transparent, abrasion-resistant antistatic coat with tin-oxide powder on plastic mouldings
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.