מחשבון מעבר לחלון LIDAR

How much signal does the cover window lose for a 905 nm or 1550 nm LiDAR?

חשב את רווח המעבר הדו-כיווני בהוספת ציפוי AR של Kriya לחלון כיסוי LIDAR ב-905, 940 או 1550 ננומטר.

How it works

A LiDAR cover window sees the emission pulse twice — once outbound, once on the return. Each pass is attenuated by the coated window's transmittance at the laser wavelength, so the signal returned to the detector scales as the square of the single-pass transmittance. A narrow-band anti-reflection coating recovers most of the loss at the design wavelength.

Worked example

Lossless incoherent slab, n 1.52: R_total = 2R / (1 + R)

Inputs: nSlab = 1.52

Result: 8.168 %

Reference: Born & Wolf §1.6.3 — thick-slab incoherent sum

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#lidar-window

Request accessOpen the interactive tool