How do I invert an ellipsometry spectrum to get n, k and thickness?
התאם מקדם שבירה n(λ), דעיכה k(λ) ועובי d מנתוני Ψ, Δ של אליפסומטריה ספקטרוסקופית. זווית יחידה או רב-זווית.
How it works
Spectroscopic ellipsometry measures the amplitude ratio (Ψ) and phase difference (Δ) between s- and p-polarised reflections from a sample. Fitting these two quantities over wavelength to a parametric optical model yields the refractive index, extinction coefficient and layer thickness. Over-parameterised models are regularised by constraining the dispersion to a physically motivated form.
Worked example
Synthetic Cauchy film on BK7
Multi-angle Ψ/Δ inversion with a 3-term Cauchy film + Urbach k on a BK7 substrate.
Validation method, references and test-case results: /validation#ellipsometry