Technology Platform

PFAS-Free Optical Coatings

Every Kriya product code can be supplied PFAS-free. That covers anti-reflective, low and high refractive index, hard coat, antistatic and solar-control coatings, from RI 1.16 to 2.00, wet-coated on film, sheet and glass and made in the Netherlands. Only for anti-fouling and easy-to-clean functions do we offer both a PFAS-based and a PFAS-free version, and the customer chooses.

What we supply PFAS-free

One supplier for the whole optical stack, so a PFAS-free requirement doesn't mean qualifying five vendors.

  • Anti-reflective coatings: single and multi-layer AR on PET, PC, PMMA, TAC and glass — AR on polymer film.
  • Low refractive index coatings, down to n = 1.16: overcoatable, for AR, waveguide cladding and light guides — low-RI coatings.
  • High refractive index nanoparticle dispersions, up to n = 2.00: for HRI layers, NIL resins and index matching — nanoparticle dispersions.
  • Hard coats: 3H–4H pencil hardness on polymer film and sheet — foldable display hardcoat.
  • Antistatic coatings: for lenses, covers and film handling — product catalogue.
  • Solar-control (ATO) coatings and dispersions: near-infrared absorption for glazing — solar heat control.
  • Anti-fouling and easy-to-clean: available in a PFAS-free version and a PFAS-based version — you choose. See the product catalogue.

Why PFAS-free matters now

The European Chemicals Agency (ECHA) has proposed the most comprehensive restriction on per- and polyfluoroalkyl substances (PFAS) ever attempted. If adopted, the restriction will phase out PFAS across nearly all industrial applications in the EU, with limited time-bound derogations. For coating formulators and their OEM customers, this is not a distant regulatory exercise — it is an imminent supply-chain event that demands material substitution now.

PFAS compounds have been the backbone of low-surface-energy coatings for decades. In optical applications, fluorinated materials deliver the low refractive indices needed for the topcoat layers of anti-reflective stacks. The challenge has always been clear: how do you achieve RI values below 1.30 without fluorine chemistry?

How conventional AR coatings depend on PFAS

Traditional anti-reflective coatings achieve low reflection through a multi-layer stack of alternating high and low refractive index materials. The low-RI topcoat — typically the most critical optical layer — has historically relied on fluorinated polymers or fluorosilanes to reach RI values in the 1.30 to 1.38 range. These materials are classified as PFAS under the ECHA proposal.

Removing PFAS from just the topcoat is insufficient if the entire stack relies on fluorinated processing aids, surfactants, or intermediates. A truly PFAS-free AR system must be PFAS-free throughout — from synthesis to final cure.

Kriya's PFAS-free RI platform

Kriya's refractive index platform covers RI 1.16 to 2.00 without PFAS, across four chemistry families:

  • Solvent sol-gel (RI 1.16 to 2.00) — cured at 200 to 700 degrees Celsius, suitable for glass and high-temperature-stable substrates
  • 100% solids UV-curable (RI 1.34 to 1.65) — solvent-free formulations for R2R and nanoimprint lithography
  • Solvent UV-curable hybrids (RI 1.35 to 1.95) — versatile multi-layer AR stacks via gravure, slot die, or spin coating
  • Thermal-curable latex (RI 1.36 to 1.50) — broad compatibility with nearly any known application method

The key breakthrough is the overcoatable PFAS-free low-RI coating reaching RI 1.16 — a value previously achievable only with fluorinated chemistry. This enables full multi-layer AR stacks entirely free from PFAS, without sacrificing the optical performance that OEMs require.

PFAS-free AR performance on polymer substrates

Kriya's PFAS-free AR coatings have been validated on four polymer substrates commonly used in display, automotive, and consumer electronics applications:

SubstrateTransmission (%)Gain (%)Haze (%)Reflection avg (%)Pencil hardnessAdhesion (%)
PET93.8+3.30.661.73H100
PC95.1+3.10.061.3HB100
PMMA96.2+2.20.761.44H100
TAC96.3+2.30.161.43H100

Basecoat thickness approximately 3.0 micrometres, topcoat approximately 0.10 micrometres. Reflection further reducible via additional layers.

Application compatibility

The PFAS-free platform serves multiple application verticals without reformulation:

  • Displays — anti-reflective films for LCD, OLED, and foldable displays. Multi-functional variants add anti-smudge, anti-static, or hardcoat properties to the AR stack. Explore display applications.
  • Automotive — HUD anti-ghosting, LIDAR window AR, and interior decorative trims with optical windows for sensors. Explore automotive optics.
  • AR/VR waveguides — high-RI core and low-RI cladding layers for diffractive waveguides. Explore waveguide applications.

Processing and integration

Kriya's PFAS-free coatings are compatible with all major wet-coating methods used in volume production:

  • Spin coating for R&D and small-batch production
  • Dip coating for cylindrical or complex geometries
  • Roll-to-roll (R2R) gravure and slot-die for high-volume film production
  • Spray coating for large-area substrates

The coatings integrate into existing production lines without equipment modification. Solvent systems are compatible with standard coating-line exhaust and recovery infrastructure. UV-curable grades eliminate solvent handling entirely.

Frequently asked questions

Is everything Kriya makes PFAS-free?

Every product code can be supplied PFAS-free. For anti-fouling and easy-to-clean functions we offer a PFAS-based and a PFAS-free version, because some customers still specify the fluorinated performance. All other functions — AR, low-RI, high-RI, hard coat, antistatic and solar control — are PFAS-free by default.

Can you replace a fluorinated coating we use today?

Usually, yes. Send us the substrate, the coating method and the target values (RI, reflection, hardness, contact angle). We formulate a PFAS-free match, send samples, and quote once you have tested them.

What RI range is available without PFAS?

RI 1.16 to 2.00, covering the full range needed for single-layer and multi-layer AR stacks. The low end (RI 1.16) was the most difficult to achieve without fluorine chemistry and represents a unique capability globally.

Can the low-RI coating be overcoated?

Yes. Unlike many low-RI materials that resist further coating adhesion, Kriya's LRI at RI 1.16 is fully overcoatable — enabling complex multi-layer stacks where the low-RI layer is not necessarily the topcoat. See the LRI coating page for details.

What is the timeline for EU PFAS restriction?

ECHA published the restriction proposal in early 2023, with RAC and SEAC opinions expected through 2025 to 2026. Adoption is anticipated in the 2025 to 2027 window, with transition periods of 18 months to several years depending on the application sector. The prudent approach is to qualify alternatives now rather than depend on derogation timelines.

How does wet-coat AR compare to vacuum-deposited AR?

Vacuum deposition (sputtering, evaporation) delivers excellent optical performance but is limited to rigid substrates and batch processing. Wet-coat AR — Kriya's approach — works on flexible polymer films, enables R2R processing, and reduces cost per square metre significantly. For polymer substrates like PET and TAC, wet-coat is the only practical path to volume.

Replace a fluorinated coating

Tell us your substrate, coating method and targets. We formulate a PFAS-free match and send samples for your own tests.