Displays — Foldable

Single-layer hardcoat passes 200,000 fold cycles with PFAS-free anti-smudge

A major Korean display Tier-1

מדדים מרכזיים

200kFold cycles passed
3HPencil hardness
2,000xSteel wool cycles passed
>95°WCA after abrasion

01

האתגר

The OEM required a multi-functional coating for foldable displays that combined hard coating, antistatic, and antifouling properties in a single layer. The coating had to survive 200,000 fold cycles at 1.5R radius without cracking or loss of surface properties, and had to be PFAS-free to meet upcoming regulatory requirements.

02

הגישה שלנו

Kriya formulated a UV-curable multi-functional coating (35 wt% solids) on 75 µm PET, combining hard coating, antistatic (10⁹ Ω/sq), and antifouling (WCA 110°) in a single layer. The coating was validated through exhaustive QC including 2,000-cycle steel wool abrasion, ballpoint pen drop tests, and permanent marker wipe-off testing.

03

התוצאה

The coating passed all qualification criteria: pencil hardness 3H, surface resistivity 8.0×10⁹ Ω/sq, WCA retained above 95° after 2,000 steel wool cycles at 1 kg/cm², and permanent marker wipe-off confirmed. The coating passes 200,000 fold cycles at 1.5R, compatible with R2R processing for volume production.

למה Kriya

Kriya delivered three functions in one PFAS-free layer, eliminating separate coating steps and reducing both processing cost and regulatory risk for the OEM’s foldable product line.

מדדים מרכזיים

200kFold cycles passed
3HPencil hardness
2,000xSteel wool cycles passed
>95°WCA after abrasion