כל מקרי הבוחן
Displays — Foldable

PFAS-free flexible AR achieves WCA >100° with better retention than PFAS

A major Korean display Tier-1

מדדים מרכזיים

>100°Water contact angle (PFAS-free)
SuperiorWCA retention vs PFAS
PassAnti-smudge durability
R2RProduction compatible

01

האתגר

With PFAS regulation tightening globally, the display OEM needed a PFAS-free anti-reflective and anti-fouling solution for foldable displays that could match or exceed the surface property retention of incumbent PFAS-based coatings under repeated mechanical stress.

02

הגישה שלנו

Kriya’s PFAS-free ARAF technology, based on functionalised HSiO₂ nanoparticles, was tested against PFAS-based references for water contact angle, anti-smudge durability, and retention after steel wool abrasion cycles. The formulation was designed for UV cure compatibility with R2R processing.

03

התוצאה

The PFAS-free coating achieved WCA above 100° with superior retention versus PFAS-based alternatives after repeated abrasion. Anti-smudge properties (fingerprint resistance and marker wipe-off) were maintained across the full test protocol. The coating is R2R-compatible for volume production.

למה Kriya

Kriya provides a complete PFAS-free alternative that actually outperforms PFAS on durability retention, eliminating regulatory risk while improving product performance.

מדדים מרכזיים

>100°Water contact angle (PFAS-free)
SuperiorWCA retention vs PFAS
PassAnti-smudge durability
R2RProduction compatible

מוצרים בשימוש

יישום קשור

Displays — Foldable →

דונו ביישום דומה

הצוות הטכני שלנו יכול לעזור לכם להעריך האם גישה זו חלה על הדרישות הספציפיות שלכם. מהיתכנות ראשונית ועד קנה מידה של ייצור.

התחילו שיחה