Automotive Thermal

16 km additional EV range through solar heat control glazing

For an EV car model, a study was carried out

מדדים מרכזיים

+16 kmRange extension (premium segment)
€325Battery saving per vehicle
35%AC power reduction
100%5G/RF/LiDAR transparent

01

האתגר

The EV manufacturer needed to extend vehicle range without increasing battery size, which adds weight and cost. AC power consumption in warm climates was identified as a significant parasitic load, particularly during the regulatory shift toward stricter EU CO₂ targets that penalise each g/km above target at €95 per vehicle.

02

הגישה שלנו

Kriya’s ATO solar heat control glazing was modelled for the premium EV segment (85.6 kWh average battery, 442 km WLTP range). The integration blocks 250 W/m² of NIR solar radiation while remaining fully transparent to 5G, RF, and LiDAR signals—a critical requirement that ITO-based alternatives cannot meet.

03

התוצאה

The analysis showed up to 16 km range extension, 8.5 kg battery saving equivalent to approximately €325 per vehicle, and 35% AC power reduction. For the compact segment (39.3 kWh, 227 km), the extension was 7 km with 4.6 kg battery saving worth approximately €159.

למה Kriya

Unlike ITO alternatives, Kriya ATO does not block RF signals, making it the only viable solar heat control solution for connected and autonomous vehicles.

מדדים מרכזיים

+16 kmRange extension (premium segment)
€325Battery saving per vehicle
35%AC power reduction
100%5G/RF/LiDAR transparent