Display coatings – Hydrophobic, Anti fouling (Anti graffiti, Hydrophobic) WCA
Kriya’s AFHC is a medium to high solids, solvent based, UV curable coating for transparent substrates. This product is developed mainly for plastic sheets and roll-to-roll film such as PET, TAC, PC, PMMA, TPU and others. The cured coating combines a high optical clarity, high water and oil contact angle, anti-fouling, and thus easy-to-clean property as well as an extreme abrasion resistant functionality.
A frequently asked combination of antistatic and easy-to-clean/ antifouling coating is available as a one pot system.
Type | PET | TAC | PC | PMMA | Glass | Steel etc. |
---|---|---|---|---|---|---|
Organic | WCA>110 | WCA>110 | WCA>110 | WCA>110 | ||
Inorganic | WCA>110 | WCA>110 |
0 = Standard | X = Optional additional feature
Type | Scratch resistance | Overcoatable | Chemical resistance | Anti static | Near Infra Red |
---|---|---|---|---|---|
Organic | 0 | 0 | X | ||
Inorganic | 0 | 0 | X |
0 = Standard | X = Optional additional feature
Kriya Materials always develops custom formulations meeting the most stringent requirements of our customers. The result is a plug and play product designed for optimal performance at the lowest total system cost.
Since we work custom based, we love to hear more about your substrate of interest and envisioned functionalities.
Please contact us through submitting our intake form.
Coatings for other substrates can be requested @ Kriya Materials
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.